Monday, August 30, 2010

Wadd?

To wadd or not?
For me, the answer is just a line of reasoning. Even well washed kiln shelves can accidentally make short work of a beautiful piece. The spot of extra time it takes to go through the steps of making the wadding, wadding up everything that's at risk, and knocking off wads and cleaning up the foot, is well worth the effort if I came come out the other end with something I can proudly put in front of a collector, gallery owner, or local customer.


Otherwise I have to shuffle my feet when customers see this... a chipped foot!







We knew that this was labor intensive when we took the job, Eh?

Tuesday, August 24, 2010

Cone 6 Wadmore

This next weekend's firing opportunity seems like a great time to explore using wads for a cone 6 firing, lifting the work up off the shelves for better heat convection in a gas kiln.


 700 grams of cone 10 clinker slop, (recycled cone 10 clay).


50 grams Alumina Hydrate...


Saw dust... (add and mix in until the slop becomes wedgable, then wedge-it up, divide it, and wrap up the batch for damp box storage.)


This may or may not go unsaid... apply small wads to the bottom of wear by dipping wads lightly in wood glue thinned with a spot of water.  This is enough wadding for a very liberal application in (2 to 3) 17 cubic foot kiln loads of work.